版权说明 操作指南
首页 > 成果 > 详情

CMAS corrosion resistance of Y2O3–Al2O3 binary ceramic materials

认领
导出
Link by DOI
反馈
分享
QQ微信 微博
成果类型:
期刊论文
作者:
Chenguang Li;Chenbiao Lai;Yaoyan Wu;Hanxiang Ouyang;Junbin Sun;...
通讯作者:
Junbin Sun<&wdkj&>Weihong Lu
作者机构:
[Chenguang Li; Chenbiao Lai] College of Chemistry and Material Science, Hengyang Normal University, Hengyang, 421008, PR China
[Yaoyan Wu; Hanxiang Ouyang] College of Nanyue, Hengyang Normal University, Hengyang, 421008, PR China
Hunan Province Key Laboratory of Functional Metal-Organic Compounds (Hengyang Normal University), Hengyang, 421008, PR China
Key Laboratory of Organometallic New Materials (Hengyang Normal University), College of Hunan Province, Hengyang, 421008, PR China
Hunan Engineering Research Center for Monitoring and Treatment of Heavy Metals Pollution in the Upper Reaches of Xiangjiang River (Hengyang Normal University), Hengyang, 421008, PR China
通讯机构:
[Junbin Sun; Weihong Lu] C
College of Chemistry and Material Science, Hengyang Normal University, Hengyang, 421008, PR China<&wdkj&>Hunan Province Key Laboratory of Functional Metal-Organic Compounds (Hengyang Normal University), Hengyang, 421008, PR China<&wdkj&>Key Laboratory of Organometallic New Materials (Hengyang Normal University), College of Hunan Province, Hengyang, 421008, PR China<&wdkj&>Hunan Engineering Research Center for Monitoring and Treatment of Heavy Metals Pollution in the Upper Reaches of Xiangjiang River (Hengyang Normal University), Hengyang, 421008, PR China
语种:
英文
期刊:
Ceramics International
ISSN:
0272-8842
年:
2024
卷:
50
期:
8
页码:
13721-13731
机构署名:
本校为第一且通讯机构
院系归属:
化学与材料科学学院
摘要:
Alumina based rare earth oxides ceramic materials, with the good performance against the CMAS corrosion, were widely used as the thermal/environmental barrier coatings. In this work, three Y2O3–Al2O3 binary ceramic bulks, which were the Y3Al5O12, YAlO3 and Y4Al2O9, were prepared by high temperature solid state reaction using the Y2O3 and Al2O3 as the raw materials. The resistances to CMAS corrosion of these materials at 1250 °C and 1350 °C were compared fully. The compositions and structures of the samples before and after corrosion were ana...